• Aqueous dispersion, 250 ml
  • Solvent: Distilled water
  • Concentration: 1-50 mg/ml
  • Flake size: 10-100 microns
  • Thickness: 1 atomic layer - no less than 80% (at a concentration of 1 mg/ml).
  • Color: Dark brown
  • Smell: No contact
  • Suspensibility: Water, ammonia water, aqueous ethanol, N-methylpyrrolidone, dimethyl sulfoxide, dimethyl formamide
  • Composition:
  • С – 46 wt.%
  • О – 49 wt.%
  • Н – 2,5 wt.%
  • S – 2.5 wt.%
  • Other impurities – <0.1 wt.%

Dispersion in Water: Single Layer Graphene Oxide (250 ml)

$0.00Price

    Download datasheet of the graphene oxide (dispersion  in water)

    Download datasheet of the reduced graphene oxide (high porosity) 

    Download datasheet of the reduced graphene oxide (nanoporosity) 

    Contact Us

     

    GraphenOx LLC

    1 Academician Semenov ave., 142432 Chernogolovka, Moscow region, Russia

    info@graphenox-ru.com

    Tel: +7(967)-160-22-96

    +7(905)-562 -06-72

    • Facebook Black Round
    • Twitter Black Round
    • YouTube - Black Circle

    The project is supported by the Innovation Promotion Fund (№2238ГС1/36985) 

    This site was designed with the
    .com
    website builder. Create your website today.
    Start Now